producten
DETAILS VAN DE PRODUCTEN
Huis > Producten >
Uitstekende weerstand tegen corrosie door spleten en stresscorrosie door kraken met Hastelloy C276/Inconel 276/2.4819 Nut

Uitstekende weerstand tegen corrosie door spleten en stresscorrosie door kraken met Hastelloy C276/Inconel 276/2.4819 Nut

MOQ: TBD
Standard Packaging: Packed with waterproof paper or weave bag, into pallets or wooden case. Special packaging requirements can also be accommodated.
Delivery Period: 7 days
Betalingswijze: T/T, D/P
Supply Capacity: 30 Tons per day
Detailinformatie
Place of Origin
China
Merknaam
Senphus
Certificering
ISO9001
Model Number
Hastelloy alloy C276/Inconel 276/Inconel 276/2.4819
Name:
Hastelloy C-276 nut
Place of Orig:
China
Type:
Hastelloy
Density:
8.9 g/cm³
Melting range:
1325-1370 ℃
Tensile strength Rm:
690 N/mm²
Yield strengthRP 0.2:
283 N/mm²
Elongation A5:
40%
Markeren:

2.4819 Noot

,

Pitting Crevice Corrosion Nut

,

Inconel 276 noten

Productomschrijving

Uitstekende weerstand tegen corrosie door spleten en stresscorrosie door kraken met Hastelloy C276/Inconel 276/2.4819 Nut

 

Hastelloy C276 (ook bekend als Inconel 276 of 2.4819) noten zijn hoogwaardige bevestigingsmiddelen gemaakt van een nikkel-molybdeen-chroom legering met uitstekende corrosiebestendigheid.Ze weerstaan zware omgevingen.Deze noten zijn bestand tegen pitting, spleet corrosie,en spanningscorrosie-crackingHastelloy C276 noten behouden mechanische sterkte en stabiliteit tot 1000°C (1832°F).Hun superieure weerstand tegen chloride-geïnduceerde aanvallen maakt ze geschikt voor offshore- en ontziltingsprojectenGemeenschappelijke normen zijn ASTM B574 en DIN 2.4819Deze moeren zijn verkrijgbaar in hex-, heavy-hex- en andere configuraties, zodat ze veilig kunnen worden bevestigd in extreme omgevingen die duurzaamheid en betrouwbaarheid vereisen.

 

Handelscode

GB ISC Verkoopcode UNS DIN EN/ DIN - Nee, nee. BS EN/BS
NS 3304
(NS 334)
(00Cr15Ni60Mo16W5Fe5)
H10276
(H 03304)
Inconel 276
Inconel C-276
N 10276 NiMo16Cr15W 2.4819 NA 45

 

 

Chemische samenstelling Wt. % % Ni Cr Fe C Deeltjes - Jawel. Mo. V P S Co. W
Min. Bal. 14.5 4       15         3.0
Maximaal Bal. 16.5 7 0.01 1.0 0.08 17 0.35 0.04 0.03 2.5 4.5

 

Fysieke constanten Dichtheid ((g/cm3) 8.9
Smeltbereik ((°C) 1325-1370

 

Minimale mechanische eigenschappen van een legering bij kamertemperatuur Typische mechanische eigenschappen Treksterkte Rm N/mm2 Kracht van het vermogen RP 0,2 N/mm2 Verlenging A5 %
Behandeling met oplossing 690 283 40

 

 

Hastelloy C276 (ook bekend als Inconel 276 of 2.4819) noten worden veel gebruikt in extreme omgevingen vanwege hun uitzonderlijke corrosiebestendigheid en hoge prestatie eigenschappen.

 

De belangrijkste kenmerken zijn:

1. Corrosiebestendigheid

  • Uitstekende weerstand tegensterk oxiderende en reducerende omgevingen
  • Uitstekende weerstand tegenpitting, scheurcorrosie en spanningscorrosie-cracking
  • Het presteert goed inzuurstoestand(zwavelzuur, zoutzuur, fosforzuur, enz.)
  • Weerstand tegen corrosiechloriderijke omgevingenen zeewater

2. Hoogtemperatuurprestaties

  • Behoudt sterkte en stabiliteit tot1,090°C (2.000°F)
  • Goed bestand tegenoxidatie en carburisatiebij hoge temperaturen

3. Mechanische sterkte

  • Hoogtrek- en opbrengststerktein vergelijking met standaard roestvrij staal
  • Uitstekend.vermoeidheidsweerstandonder cyclische belastingomstandigheden

4Chemische samenstelling

  • Voornamelijk samengesteld uit:Nikkel (Ni) (~ 57%), met toevoegingen vanMolybdeen (Mo) (~ 16%),Chroom (Cr) (~ 15,5%), enIJzer (Fe) (~5-7%)
  • Een laag koolstofgehalte minimaliseert de carbide neerslag tijdens het lassen

 

 

Hastelloy C276 (ook bekend als Inconel 276 of 2.4819) noten worden veel gebruikt in industrieën die uitzonderlijke corrosiebestendigheid en hoge mechanische sterkte vereisen.

 

Hier zijn de belangrijkste toepassingen:

1Chemische verwerkende industrie

  • Gebruikt in reactoren, warmtewisselaars en leidingsystemen die zeer corrosieve chemicaliën behandelen zoals zoutzuur, zwavelzuur en chloor.
  • Ideaal voor het bevestigen van onderdelen in agressieve chemische omgevingen.

2Maritieme en offshore-industrie

  • Ze zijn bestand tegen zeewater en pekelwater, waardoor ze geschikt zijn voor offshoreplatforms, scheepsbouw en onderwatertoepassingen.
  • Gebruikt in ontziltingsinstallaties en mariene warmtewisselaars.

3. Lucht- en ruimtevaart

  • Gebruikt in uitlaatsystemen van vliegtuigen, straalmotoren en andere gebieden met hoge temperaturen waar oxidatie- en corrosiebestendigheid cruciaal zijn.

4. Energiecentrales

  • Gevonden in kerncentrales, ontzwavelingssystemen voor rookgassen (FGD) en geothermische energiecentrales vanwege hun weerstand tegen zwavelverbindingen en zure gassen.

5. Pulp- en papierindustrie

  • Gebruikt in blekingsapparatuur en digestoren waar sterke zuren en chloorverbindingen aanwezig zijn.

6. Farmaceutische en voedselverwerkende industrie

  • Geschikt voor omgevingen waar verontreiniging moet worden vermeden en waar agressieve reinigingsmiddelen worden gebruikt.

7. Afvalverwerkingsinstallaties

  • Gebruikt in afvalverbrandingsinstallaties en afvalwaterzuiveringsinstallaties vanwege hun bestandheid tegen ruwe en corrosieve afvalomgevingen.

Uitstekende weerstand tegen corrosie door spleten en stresscorrosie door kraken met Hastelloy C276/Inconel 276/2.4819 Nut 0Uitstekende weerstand tegen corrosie door spleten en stresscorrosie door kraken met Hastelloy C276/Inconel 276/2.4819 Nut 1Uitstekende weerstand tegen corrosie door spleten en stresscorrosie door kraken met Hastelloy C276/Inconel 276/2.4819 Nut 2

producten
DETAILS VAN DE PRODUCTEN
Uitstekende weerstand tegen corrosie door spleten en stresscorrosie door kraken met Hastelloy C276/Inconel 276/2.4819 Nut
MOQ: TBD
Standard Packaging: Packed with waterproof paper or weave bag, into pallets or wooden case. Special packaging requirements can also be accommodated.
Delivery Period: 7 days
Betalingswijze: T/T, D/P
Supply Capacity: 30 Tons per day
Detailinformatie
Place of Origin
China
Merknaam
Senphus
Certificering
ISO9001
Model Number
Hastelloy alloy C276/Inconel 276/Inconel 276/2.4819
Name:
Hastelloy C-276 nut
Place of Orig:
China
Type:
Hastelloy
Density:
8.9 g/cm³
Melting range:
1325-1370 ℃
Tensile strength Rm:
690 N/mm²
Yield strengthRP 0.2:
283 N/mm²
Elongation A5:
40%
Minimum Order Quantity:
TBD
Packaging Details:
Packed with waterproof paper or weave bag, into pallets or wooden case. Special packaging requirements can also be accommodated.
Delivery Time:
7 days
Payment Terms:
T/T, D/P
Supply Ability:
30 Tons per day
Markeren

2.4819 Noot

,

Pitting Crevice Corrosion Nut

,

Inconel 276 noten

Productomschrijving

Uitstekende weerstand tegen corrosie door spleten en stresscorrosie door kraken met Hastelloy C276/Inconel 276/2.4819 Nut

 

Hastelloy C276 (ook bekend als Inconel 276 of 2.4819) noten zijn hoogwaardige bevestigingsmiddelen gemaakt van een nikkel-molybdeen-chroom legering met uitstekende corrosiebestendigheid.Ze weerstaan zware omgevingen.Deze noten zijn bestand tegen pitting, spleet corrosie,en spanningscorrosie-crackingHastelloy C276 noten behouden mechanische sterkte en stabiliteit tot 1000°C (1832°F).Hun superieure weerstand tegen chloride-geïnduceerde aanvallen maakt ze geschikt voor offshore- en ontziltingsprojectenGemeenschappelijke normen zijn ASTM B574 en DIN 2.4819Deze moeren zijn verkrijgbaar in hex-, heavy-hex- en andere configuraties, zodat ze veilig kunnen worden bevestigd in extreme omgevingen die duurzaamheid en betrouwbaarheid vereisen.

 

Handelscode

GB ISC Verkoopcode UNS DIN EN/ DIN - Nee, nee. BS EN/BS
NS 3304
(NS 334)
(00Cr15Ni60Mo16W5Fe5)
H10276
(H 03304)
Inconel 276
Inconel C-276
N 10276 NiMo16Cr15W 2.4819 NA 45

 

 

Chemische samenstelling Wt. % % Ni Cr Fe C Deeltjes - Jawel. Mo. V P S Co. W
Min. Bal. 14.5 4       15         3.0
Maximaal Bal. 16.5 7 0.01 1.0 0.08 17 0.35 0.04 0.03 2.5 4.5

 

Fysieke constanten Dichtheid ((g/cm3) 8.9
Smeltbereik ((°C) 1325-1370

 

Minimale mechanische eigenschappen van een legering bij kamertemperatuur Typische mechanische eigenschappen Treksterkte Rm N/mm2 Kracht van het vermogen RP 0,2 N/mm2 Verlenging A5 %
Behandeling met oplossing 690 283 40

 

 

Hastelloy C276 (ook bekend als Inconel 276 of 2.4819) noten worden veel gebruikt in extreme omgevingen vanwege hun uitzonderlijke corrosiebestendigheid en hoge prestatie eigenschappen.

 

De belangrijkste kenmerken zijn:

1. Corrosiebestendigheid

  • Uitstekende weerstand tegensterk oxiderende en reducerende omgevingen
  • Uitstekende weerstand tegenpitting, scheurcorrosie en spanningscorrosie-cracking
  • Het presteert goed inzuurstoestand(zwavelzuur, zoutzuur, fosforzuur, enz.)
  • Weerstand tegen corrosiechloriderijke omgevingenen zeewater

2. Hoogtemperatuurprestaties

  • Behoudt sterkte en stabiliteit tot1,090°C (2.000°F)
  • Goed bestand tegenoxidatie en carburisatiebij hoge temperaturen

3. Mechanische sterkte

  • Hoogtrek- en opbrengststerktein vergelijking met standaard roestvrij staal
  • Uitstekend.vermoeidheidsweerstandonder cyclische belastingomstandigheden

4Chemische samenstelling

  • Voornamelijk samengesteld uit:Nikkel (Ni) (~ 57%), met toevoegingen vanMolybdeen (Mo) (~ 16%),Chroom (Cr) (~ 15,5%), enIJzer (Fe) (~5-7%)
  • Een laag koolstofgehalte minimaliseert de carbide neerslag tijdens het lassen

 

 

Hastelloy C276 (ook bekend als Inconel 276 of 2.4819) noten worden veel gebruikt in industrieën die uitzonderlijke corrosiebestendigheid en hoge mechanische sterkte vereisen.

 

Hier zijn de belangrijkste toepassingen:

1Chemische verwerkende industrie

  • Gebruikt in reactoren, warmtewisselaars en leidingsystemen die zeer corrosieve chemicaliën behandelen zoals zoutzuur, zwavelzuur en chloor.
  • Ideaal voor het bevestigen van onderdelen in agressieve chemische omgevingen.

2Maritieme en offshore-industrie

  • Ze zijn bestand tegen zeewater en pekelwater, waardoor ze geschikt zijn voor offshoreplatforms, scheepsbouw en onderwatertoepassingen.
  • Gebruikt in ontziltingsinstallaties en mariene warmtewisselaars.

3. Lucht- en ruimtevaart

  • Gebruikt in uitlaatsystemen van vliegtuigen, straalmotoren en andere gebieden met hoge temperaturen waar oxidatie- en corrosiebestendigheid cruciaal zijn.

4. Energiecentrales

  • Gevonden in kerncentrales, ontzwavelingssystemen voor rookgassen (FGD) en geothermische energiecentrales vanwege hun weerstand tegen zwavelverbindingen en zure gassen.

5. Pulp- en papierindustrie

  • Gebruikt in blekingsapparatuur en digestoren waar sterke zuren en chloorverbindingen aanwezig zijn.

6. Farmaceutische en voedselverwerkende industrie

  • Geschikt voor omgevingen waar verontreiniging moet worden vermeden en waar agressieve reinigingsmiddelen worden gebruikt.

7. Afvalverwerkingsinstallaties

  • Gebruikt in afvalverbrandingsinstallaties en afvalwaterzuiveringsinstallaties vanwege hun bestandheid tegen ruwe en corrosieve afvalomgevingen.

Uitstekende weerstand tegen corrosie door spleten en stresscorrosie door kraken met Hastelloy C276/Inconel 276/2.4819 Nut 0Uitstekende weerstand tegen corrosie door spleten en stresscorrosie door kraken met Hastelloy C276/Inconel 276/2.4819 Nut 1Uitstekende weerstand tegen corrosie door spleten en stresscorrosie door kraken met Hastelloy C276/Inconel 276/2.4819 Nut 2